000 00850nam a2200157Ia 4500
008 220216s9999 xx 000 0 und d
100 _aEng A H
245 0 _aEpoxide groups in natural rubber. 1. 13C-NMR study of oxidative degraded rubbers
260 _bJournal of Rubber Research
_c1998
300 _a67-76
520 _aEpoxide groups in natural rubber, which are derived from oxidative degradation of the polymer, are found to be mainly in cis configuration. The amount of trans epoxide, on the other hand, increases with increasing degradation temperature of the natural rubber. The presence of cis epoxide groups in low molecular weight fractions of natural rubber, therefore, may be associated to by-products of oxidative degradation of the polymer.
700 _aKawahara S
700 _aTanaka Y
700 _aTandpakdee J
942 _cJS
999 _c58726