| 000 | 00750nam a2200265Ia 4500 | ||
|---|---|---|---|
| 008 | 220216s9999 xx 000 0 und d | ||
| 100 | _aYong K C | ||
| 245 | 0 | _aElectrically conductive epoxidised natural rubber-polyaniline dodecylbenzenesulfonate blends prepared by solution mixing | |
| 260 |
_bJournal of Rubber Research _c2008 |
||
| 300 | _a59-77 | ||
| 520 | _aDL | ||
| 650 | _aConductive blend | ||
| 650 | _aElectrical conductivity | ||
| 650 | _aEpoxide level | ||
| 650 | _aEpoxidised natural rubber(ENR) | ||
| 650 | _aPolyaniline | ||
| 650 | _aRing opening | ||
| 650 | _aSolution mixing | ||
| 700 | _aCook S | ||
| 700 | _aFoot P J S | ||
| 700 | _aMd Aris Ahmad | ||
| 700 | _aMorgan H | ||
| 700 | _aTinker A J | ||
| 942 | _cJS | ||
| 999 |