Effect of different paraffin waxes and antiozonant on the processing and mechanical properties of natural rubber (Record no. 57798)
[ view plain ]
| 000 -LEADER | |
|---|---|
| fixed length control field | 01841nam a2200253Ia 4500 |
| 100 ## - MAIN ENTRY--AUTHOR NAME | |
| Personal name | Kamaruddin A N |
| 245 #0 - TITLE STATEMENT | |
| Title | Effect of different paraffin waxes and antiozonant on the processing and mechanical properties of natural rubber |
| 260 ## - PUBLICATION, DISTRIBUTION, ETC. (IMPRINT) | |
| Name of publisher | Journal of Rubber Research |
| Year of publication | 2012 |
| 300 ## - PHYSICAL DESCRIPTION | |
| Number of Pages | 35-45 |
| 500 ## - GENERAL NOTE | |
| General note | Source Year: 2012 |
| 520 ## - SUMMARY, ETC. | |
| Summary, etc | Three commercial paraffin waxes (carbon numbers 20-40) and one alkyl-aryl-p-phenylene-diamine antiozonant were mixed individually with natural rubber to produce rubber compounds. The compounds contained a precipitated amorphous white silica nanofiller the surface of which was pre-treated with bis(3-triethoxysilylpropyl-) tetrasulphane (TESPT). The rubber compounds were cured via the tetrasulphane groups of TESPT by adding a sulphenamide accelerator and zinc oxide. The viscosity, cure properties, hardness, tensile strength, elongation at break, stored energy density at break, Youngs modulus, modulus at different strain amplitudes, tear strength and cyclic fatigue life of the rubber vulcanizates were measured. The viscosity, scorch time and rate of cure increased, but the optimum cure time decreased when the waxes and antioxonant were added to the rubber. The highest tensile strength, stored energy density at break, modulus at different strain amplitudes and the longest cyclic fatigue life were measured for the vulcanisate with the antiozonant. The rubber vulcanisate containing one of the waxes had the highest tear strength. |
| 650 ## - SUBJECT ADDED ENTRY--TOPICAL TERM | |
| Topical Term | Antiozonant |
| 650 ## - SUBJECT ADDED ENTRY--TOPICAL TERM | |
| Topical Term | Glycol |
| 650 ## - SUBJECT ADDED ENTRY--TOPICAL TERM | |
| Topical Term | Mechanical properties |
| 650 ## - SUBJECT ADDED ENTRY--TOPICAL TERM | |
| Topical Term | Paraffin waxes |
| 650 ## - SUBJECT ADDED ENTRY--TOPICAL TERM | |
| Topical Term | Processing properties |
| 650 ## - SUBJECT ADDED ENTRY--TOPICAL TERM | |
| Topical Term | Swelling |
| 700 ## - ADDED ENTRY--PERSONAL NAME | |
| Personal name | Ansarifar A |
| 700 ## - ADDED ENTRY--PERSONAL NAME | |
| Personal name | Ellis R J |
| 700 ## - ADDED ENTRY--PERSONAL NAME | |
| Personal name | Haile-Meskel Y |
| 700 ## - ADDED ENTRY--PERSONAL NAME | |
| Personal name | Saeed F |
| 942 ## - ADDED ENTRY ELEMENTS (KOHA) | |
| Koha item type | Journals |
| Withdrawn status | Lost status | Damaged status | Not for loan | Home library | Current library | Shelving location | Date acquired | Serial Enumeration / chronology | Koha item type |
|---|---|---|---|---|---|---|---|---|---|
| Journals | RRII Library | RRII Library | Rubber technology | 04/03/2013 | Volume 15, Issue 1 | Journals |