Image from Google Jackets

Pyrolysis of polychloroprene rubber in a fluidised-bed reactor-product composition with focus on chlorinated aromatic compounds

By: Contributor(s): Material type: TextTextPublication details: Polymer Degradation and Stability 2001Description: 39-51Subject(s): Summary: Polychloroprene rubber was pyrolysed in a fluidised-bed reactor on laboratory scale at 593 oC. The distribution of the pyrolysis products was investigated. Mass balances of all product fractions were obtained. Analytical interest was focused on the chlorinated aromatic compounds. Polycyclic aromatic compounds were found in quite high concentrations of up to 0.1;in the oil. Polychlorinated biphenyls were measured in trace levels of up to 1.8 ppm.
Tags from this library: No tags from this library for this title. Log in to add tags.
Star ratings
    Average rating: 0.0 (0 votes)
Holdings
Item type Current library Vol info Status
Journals Journals RRII Library Rubber chemistry Volume 71, Issue 1 Journals
Total holds: 0

Polychloroprene rubber was pyrolysed in a fluidised-bed reactor on laboratory scale at 593 oC. The distribution of the pyrolysis products was investigated. Mass balances of all product fractions were obtained. Analytical interest was focused on the chlorinated aromatic compounds. Polycyclic aromatic compounds were found in quite high concentrations of up to 0.1;in the oil. Polychlorinated biphenyls were measured in trace levels of up to 1.8 ppm.